inquiry
Leave Your Message

Adhesion Test Data: 3.5N/cm Performance on Recycled Cardboard

2026-10-30

TL;DR

  • Our peel adhesion result on recycled cardboard is 3.5 N/cm, and the number is only meaningful together with the five conditions it was measured under.
  • Adhesion is three different tests, not one: peel adhesion, tack and shear, and a tape can pass one and fail another without contradiction.
  • Recycled board is the hard substrate, because recycled fibre gives an uneven surface, variable surface energy and a board that can tear before the tape lets go.
  • The failure mode tells you more than the number: adhesive, cohesive and substrate failure each point to a different fix.
  • Ask a supplier for the standard, the substrate, the coat weight, the dwell time and the conditioning, because without those five a figure cannot be compared with anybody else's.

"A packaging film that outlasts the product it protects is not a packaging solution — it is a waste problem waiting to happen." That is the position I have held since I joined Zhejiang Xiade New Material in 2010 and started working on natural cellulose films that meet EU food contact material standards, and it is also why adhesion data on recycled board matters more than most people expect.

In my experience, cellulose is a different substrate from polyethylene film, and recycled cardboard is a different substrate again. A tape that peels at 3.5 N/cm from recycled board may behave very differently on virgin kraft, on coated carton or on a woven PP sack, and the reason sits in the fibre, the adhesive chemistry and the surface energy of what you are sticking to.

This guide walks through the measurement itself: which adhesion test you are actually buying, the conditions that have to travel with the number, why recycled board is the difficult case, how to read a failure mode, and what a medical device or food packaging buyer should request before approving a tape supplier. The products referenced are ours, from our biodegradable tape and cellulose film range to our biodegradable clear sealing tape.

image.png

What "Adhesion" Means and Which Test You Are Buying

Adhesion is not one property but three, and the word on a datasheet only becomes useful when you know which one it refers to.

  • Peel adhesion is how much force per centimetre of width it takes to peel the tape off the substrate at a stated angle and speed. It is quoted in N/cm or N/mm, and it is the number in this article's title.
  • Tack is how quickly the adhesive grabs the surface on first contact with very light pressure, measured by loop tack or ball tack. It decides whether a tape sticks to a dusty carton in one pass, not whether it stays there for a month.
  • Shear is how much static load the tape holds while it is not being peeled, which is what matters when a box is stacked and the seal is carrying weight.

Because a tape can have excellent tack, ordinary peel and poor shear at the same time, and because a peel figure depends on the angle it was measured at, a buyer who compares two numbers without comparing the methods is comparing two different tests. Our 3.5 N/cm is a peel figure, and it is a 180° peel, which is the most demanding geometry because it loads the adhesive edge rather than peeling the tape off flat.

How the Test Is Run

The five conditions below are not footnotes, they are the number itself.

  1. The standard and the geometry. The common references are ASTM D3330 for peel adhesion of pressure-sensitive tape, the Pressure Sensitive Tape Council's PSTC-101 methods, FINAT Test Method 2, and the Chinese GB/T 2790 series. All four exist because the results are only comparable inside one method.
  2. The conditioning. Tape and substrate are conditioned before testing, and the practice is set out in ASTM D4332. Industry practice is 23 ± 2 °C at 50 ± 5% relative humidity, because humidity changes the water content of a cellulose film and therefore changes the adhesive.
  3. The application method. The tape is applied with a specified roller and a specified pressure. Hand application varies far more than most people think, and it is the fastest way to make two results incomparable.
  4. The dwell time. Adhesion builds after application. Testing at 24 hours and testing at 72 hours on the same tape can give different numbers, and a supplier who quotes a figure without the dwell has not quoted a figure.
  5. The substrate. Recycled board is specified by its recycled content, grammage, coating or liner, and by the storage condition it came out of.

Because the test method is published and stable, the fastest way to make two suppliers comparable is to require the same method, the same conditioning and the same dwell, and only then compare the numbers.

Why Recycled Cardboard Is the Difficult Substrate

Recycled board fails in three ways that virgin kraft does not, and knowing which one you are looking at saves weeks of formulation work.

  • Uneven surface and variable topography. Recycled fibre is shorter and less uniform than virgin kraft, so the contact area between adhesive and substrate varies across the tape, and the peel path becomes irregular.
  • Variable surface energy. Adhesion to paper is largely mechanical and hydrogen-bonding based, so residues, inks, adhesives and contaminants left in the recycling stream directly affect how the tape anchors.
  • The board can tear before the tape lets go. On a weak recycled liner, a high peel force can be achieved simply by the board splitting, which looks like excellent adhesion in a tensile test and is a complete failure in a carton.

Because a recycled board can tear before the adhesive releases, the failure mode has to be read, not just the force, and I would not approve a tape on a number alone.

The 3.5 N/cm Figure and the Conditions It Travels With

Our own peel adhesion result on recycled cardboard is 3.5 N/cm, measured as a 180° peel in the conditions described above, and I publish it with those conditions attached because a figure without them is not a specification.

Put the number into packaging terms, because that is how a buyer uses it. At 3.5 N/cm, a 48 mm wide strip carries about 16.8 N of peel force across its width, which means a seal length has to be long enough for the peel force to stay below the stress the board can take, and the same arithmetic works in reverse for comparing a narrower tape on a heavier board. The practical consequence is that a 3.5 N/cm tape can be entirely adequate for a light duty pouch and marginal for a heavy duty corrugated shipper, and the deciding variable is usually the board, not the tape.

Because the same tape, the same roll and the same batch can produce different numbers on different board, I would treat any comparison that does not state the substrate as a comparison of nothing.

Reading the Failure Mode

When the tape comes off, look at what is left behind, because that single observation tells you more than the number does.

  • Adhesive failure. The tape releases cleanly and the adhesive stays on the board, which means the bond to the substrate was weaker than the internal strength of the adhesive layer. The fix is usually a different chemistry or a different coat weight.
  • Cohesive failure. The adhesive splits and strings between the tape and the board, which means the adhesive layer was internally strong but the peel rate was faster than the layer could resist. It usually means the peel was too fast, the peel angle wrong, or the adhesive too soft for the temperature.
  • Substrate failure. The board surface tears and the tape stays on the carton, which means the interface was excellent and the board was the weak link. This is the failure mode that is easiest to misread as good performance.

Because a supplier who photographs the failed bond tells you more in one image than a table of numbers does, I ask for a photograph of the failure for every substrate we qualify.

Food Contact, Barrier and Compostability in the Same Decision

For medical device and food packaging buyers, adhesion is only one of three requirements the same tape has to satisfy.

In Europe, the framework for materials intended to come into contact with food is Regulation (EC) No 1935/2004, and plant-fibre-based materials sit inside it. Our natural cellulose film has been developed to meet the EU food contact material standards, and the same substrate brings the properties those applications ask for: a biodegradable film that is also heat resistant, insulating and anti-static, which is why the same base material serves packaging, tape substrates and insulation.

The tension a buyer has to manage is real: the adhesive has to hold on a surface that is designed to disappear. A compostable or biodegradable substrate has no use if the pack it seals is still intact after its shelf life, and a film that outlasts what it protects is exactly the waste problem I quoted at the top. That is why compostability specifications such as EN 13432 for industrial composting and EN 17033 for home composting should be read together with the sealing requirement and the intended shelf life, not separately from them.

Because the barrier, the seal and the end-of-life route are decided together, I would rather specify a tape against a complete application profile than against a single adhesion figure.

What to Ask a Supplier Before You Approve a Tape

Eight items, and a supplier who answers all eight has given you a specification rather than a brochure.

  • The test method and peel geometry, with the standard number: ASTM D3330, PSTC-101, FINAT TM2 or GB/T 2790.
  • The conditioning, in temperature and relative humidity, per the conditioning practice used.
  • The application method, including roller pressure and width of application.
  • The dwell time between application and test.
  • The substrate description, including recycled content, grammage, liner or coating and storage history.
  • The adhesive coat weight in grams per square metre, because adhesion scales with it.
  • A failure-mode photograph for the substrate you actually use.
  • Food contact documentation for your market, and lot-level traceability for the roll.

Our own position is straightforward: every roll on our biodegradable clear sealing tape goes through quality control checks, the tape is offered in custom widths, lengths and colours with printed logos, and we supply the documentation package to go with it. Because an approval conversation that starts with the substrate ends faster than one that starts with the tape, my first question to any buyer is what the board is and how it was stored.

Frequently Asked Questions

What does 3.5 N/cm mean for a cellulose tape on recycled cardboard?

It is a peel adhesion figure, meaning roughly 3.5 newtons per centimetre of tape width at 180°, so a 48 mm strip carries about 16.8 N across its width. It says nothing about tack or shear, and it only holds on the substrate and under the conditioning, application and dwell conditions it was measured with.

Why is recycled cardboard harder to stick to than virgin kraft?

Recycled fibre is shorter and less uniform, so the contact area varies and the surface topography is irregular. Residues, inks and adhesives left in the recycling stream change the surface energy the adhesive has to anchor to, and a weak recycled liner can tear before the adhesive lets go.

How do I know whether a tape failed because of the adhesive or because of the board?

Look at what is left on the board. If the tape releases cleanly and the adhesive stays behind, the bond was weaker than the adhesive layer. If the adhesive strings and splits, the layer was internally strong but peeled too fast. If the board surface tears and the tape stays on the carton, the interface was fine and the board was the weak link.

Does the peel angle change the adhesion figure?

Yes, substantially, which is why it has to be stated. A 180° peel loads the adhesive edge and normally reads lower than a 90° peel on the same tape and substrate. It is also why a 3.5 N/cm figure cannot be compared with a figure measured at a different angle, even when everything else matches.

Can a compostable tape still seal a pack properly?

Yes, provided the sealing requirement and the end-of-life route are specified together. Cellulose-based tapes can deliver strong adhesion and, at the same time, a film that breaks down under industrial composting conditions such as EN 13432 or home composting conditions under EN 17033. What matters is that the shelf life of the pack is shorter than the persistence of the film that seals it.

Where the Decision Belongs

Adhesion data is a specification, not a marketing number, and the difference shows up the moment somebody tries to compare two rolls without knowing which board they came from.

I work with medical device and food packaging buyers who have to balance barrier performance, sterilization compatibility and EU sustainability requirements at industrial scale, and that is exactly where adhesion figures get used carelessly. Send me the substrate, the sealing application and the market, and I will come back with the adhesion data measured under conditions you can specify and defend, plus the documentation package your file will need.

Yusheng Yan

Senior Materials Scientist & Technical Director, Zhejiang Xiade New Material Co., Ltd. (XIADE)

I joined XIADE in 2010 and have worked on the research and development of natural cellulose films that meet EU food contact material standards. These films are biodegradable, insulating, heat-resistant and anti-static, and they serve aerospace, military, medical subcontracting, food subcontracting, craft packaging, tape substrates and insulation materials. Zhejiang Xiade New Material operates from the largest ecological industrial park in Zhejiang, covering 116,700 square metres with a 60,000 square metre building area, and holds ISO 9001:2000 and ISO 14001:2004 certification as China's largest manufacturer of natural cellulose membranes. My work is with medical device and food packaging buyers who need to balance barrier performance, sterilization compatibility and EU sustainability requirements at industrial scale.

Facebook Request adhesion test data